Title: | Improvement of Cu-Al bond integrity on low k pad structures | Authors: | Kid, W.B. Leng, E.P. Yong, C.C. Yi, O.X. Kar, Y.B. |
Issue Date: | 2011 | Abstract: | Gold wires are commonly used for wire-bonding and it fits well the industrial requirements. However, the price of Gold wires increasing significantly, Copper wires is a potential replacement for Gold due to their superior electrical and mechanical properties. In order to incorporate Cu in the wire-bonding process, substantial data regarding aging and intermetallic formation of Cu-Al bonds is required and the results are compared with Au samples. In this study, the bond integrity and thermal aging of Cu-Al and Au-Al wire-bonds were investigated. The Copper and Gold wire-bonds samples were heat-treated at temperature of 225°C for 4.5, 13.5, 26, 52 and 97 hours respectively. The intermetallics of the wire-bonds, and in particular the Al-Cu interface, were studied. Discontinuous and non-uniform of Cu-Al intermetallics regions were found in the thermal aging samples. The thickness of Cu-Al intermetallics is growing linearly with the temperature as the diffusion rate increases in higher temperature. The Cu-Al bond is weak compare to Au-Al in accordance with aging through wire pull test. © 2011 IEEE. | URI: | http://dspace.uniten.edu.my/jspui/handle/123456789/8801 |
Appears in Collections: | COE Scholarly Publication |
Show full item record
Google ScholarTM
Check
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.